Cure Time 7200 min

@Temperature 22.0 °C
120 hour

@Temperature 71.6 °F
Dow Corning SE 4486 SILICONE RTV
One-part, white, moisture cure RTV, highly flowable, fast tack-free, high thermal conductivity, controlled volatility.Information provided by Dow Corning
Cure Time 7200 min
120 hour
3M AC-275 Class B-4 Aerospace Sealant
3M Aerospace Sealant AC-275 Class B is a high temperature two-component manganese dioxide cured, liquid polysulfide polymer sealants providing excellent fuel tank and fuselage seals. They have outst..
Cure Time 7200 min
120 hour
3M AC-730 Class B-12 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Cure Time 7200 min
120 hour
Full Cure
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild
Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abra..
Cure Time 7200 min
120 hour
Full Cure
3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer
Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.Product Features:Combines good..