Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 40.0 - 60.0 min | 0.667 - 1.00 hour | working strength |
Permabond TA430 Acrylic Adhesive & Initiator PERMABOND TA430 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics, wood, and some thermoplastics. This adhesive may be used in a variety of structural bondin.. |
|||
Cure Time | 40.0 min | 0.667 hour | Fixture |
Resinlab® RC8040 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Cure Time | 40.0 min @Temperature 141 °C |
0.667 hour @Temperature 285 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 40.0 - 45.0 min | 0.667 - 0.750 hour | Fixture time |
ITW Devcon Flex Welderâ„¢ Methacrylate Adhesive, Off-White Information provided by ITW Devcon |
|||
Cure Time | 40.0 min | 0.667 hour | Tack Free Time |
Shin-Etsu Silicones KE-44 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | 40.0 min @Temperature 141 °C |
0.667 hour @Temperature 285 °F |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 40.0 min @Temperature 121 °C |
0.667 hour @Temperature 250 °F |
|
Tra-Con Tra-Duct 921U01 Information provided by Tra-Con Inc. |
|||
Cure Time | 40.0 min | 0.667 hour | |
Loctite® 266 High Temperature/High Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Cure Time | 40.0 - 60.0 min | 0.667 - 1.00 hour | Tack-Free, 50% RH |
3M 740 Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Cure Time | 40.0 - 70.0 min | 0.667 - 1.17 hour | Tack-Free, 50% RH |
3M 755 Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Cure Time | 40.0 - 60.0 min | 0.667 - 1.00 hour | handling time |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |