Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 - 960 min @Temperature 23.0 °C |
6.00 - 16.0 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Cure Time | 360 - 480 min @Temperature 25.0 °C |
6.00 - 8.00 hour @Temperature 77.0 °F |
Full Cure |
Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhe.. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5249 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 - 600 min @Temperature 23.9 °C |
6.00 - 10.0 hour @Temperature 75.0 °F |
|
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3101 Encapsulating Adhesive System TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is rec.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3104 Low Viscosity Epoxy Casting Compound TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free s.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3109 Low Cost Epoxy Casting System TRA-CAST 3109 is a versatile epoxy casting system developed for solvent-free production casting, potting, encapsulating, and coating applications where low cost, easy handling and flowability, and e.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a.. |
|||
Cure Time | >= 360 min | >= 6.00 hour | |
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | 360 - 2880 min | 6.00 - 48.0 hour | Full Cure; Unprimed |
Loctite® Gasket Eliminator® 509 Flange Sealant Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Cure Time | 360 - 480 min @Temperature 24.0 °C |
6.00 - 8.00 hour @Temperature 75.2 °F |
|
BCC Products BC 5003 Epoxy Laminating System BC 5003 is a medium viscosity, unfilled laminating system. It is a room temperature curing resin with a relatively short pot life. BC 5003 is also considered an excellent general purpose adhesive fo.. |
|||
Cure Time | 360 min | 6.00 hour | Touch Dry |
3M Scotchkote™ CR 511 Epoxy Ceramic Surface Scotchkote Epoxy Ceramic CR 511 has been specifically developed as a 100% solids coating for resurfacing and lining to improve the efficiency of equipment in fluid flow environments.Product Features.. |
|||
Cure Time | 360 min | 6.00 hour | Machining Time |
3M Scotchkote™ FG 512 Epoxy Ceramic Surfacer Scotchkote Epoxy Ceramic Surfacer FG 512 has been specifically developed as a ceramic enhanced epoxy repair coating for resurfacing and reforming metal machinery and equipment, such as pumps, impell.. |
|||
Cure Time | 360 min | 6.00 hour | Touch Dry |
3M Scotchkote™ HTX 517 Epoxy HT Lining Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a.. |
|||
Cure Time | 360 min @Temperature 24.0 °C |
6.00 hour @Temperature 75.2 °F |
demold time |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Cure Time | 360 min | 6.00 hour | Full Cure |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |
|||
Cure Time | 360 - 420 min | 6.00 - 7.00 hour | |
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 360 min | 6.00 hour | Hard Dry, 1 hr when surface temp at 50°C |
3M Scotchkote™ 162PWX Epoxy Coating 3M Scotchkote Epoxy Coating 162PWX is a 100% solid two-part epoxy coating that has been specifically developed for the long term protection of drinking water pipelines, storage and process tanks or .. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | demold time |
BCC Products BC 8860 Polyurethane Elastomer BC8860 is a low viscosity two-component urethane casting compound that is specifically formulated for high abrasion and impact resistance. It is recommended for use for the production casting of hig.. |
|||
Cure Time | 360 min | 6.00 hour | |
3M AC-730 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Cure Time | 360 - 2880 min | 6.00 - 48.0 hour | Full Cure; Unprimed |
Loctite® 573 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations |