Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 12.0 min | >= 0.200 hour | Air Set prior to curing |
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled
(discontinued **) Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe.. |
|||
Cure Time | 12.0 min @Temperature 83.3 °C |
0.200 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 12.0 min @Temperature 68.3 °C |
0.200 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 12.0 min @Temperature 68.3 °C |
0.200 hour @Temperature 155 °F |
Press cured |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 - 14.0 min | 0.200 - 0.233 hour | Working time |
ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads Information provided by ITW Devcon |
|||
Cure Time | 12.0 min | 0.200 hour | Tack Free Time |
Shin-Etsu Silicones KE-40RTV Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | 12.0 min | 0.200 hour | Tack Free Time |
Shin-Etsu Silicones KE-3417 Silicone, RTV Adhesive Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Cure Time | >= 12.0 min | >= 0.200 hour | |
Trelleborg Emerson & Cuming Stycast® 926-82-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | >= 12.0 min | >= 0.200 hour | |
Trelleborg Emerson & Cuming Stycast® 933-48 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Cure Time | >= 12.0 min | >= 0.200 hour | |
Trelleborg Emerson & Cuming Stycast® G-508-1 One-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Cure Time | 12.0 min @Temperature 68.3 °C |
0.200 hour @Temperature 155 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.25 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 83.3 °C |
0.200 hour @Temperature 182 °F |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Cure Time | 12.0 min | 0.200 hour | t'90, Target; ASTM D2084 (mod) |
ExxonMobil Chlorobutyl 1066 Rubber Product Description: Exxon™ Chlorobutyl rubber is a copolymer of isobutylene and isoprene. The product has characteristic specific gravity of 0.93. The product form is white to light amber bales.In.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.5 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBT MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Sulfur MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR Zinc Stearate MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Cure Time | 12.0 min @Temperature 160 °C |
0.200 hour @Temperature 320 °F |
Press cured |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 4.0 PHR MBTS MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |