Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 0.833 - 1.83 min | 0.0139 - 0.0306 hour | Gelation time |
Mitsui MILEXâ„¢ RS-2210MB Silicone Rubber Modified Phenolic Resin The MILEXâ„¢ Family of products is widely featured in brake systems of automobiles made by automakers through Mitsui Chemicals'. The phenolic material is primarily used as binders in brake pad.. |
|||
Cure Time | 0.833 - 1.00 min | 0.0139 - 0.0167 hour | per mm |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Cure Time | 0.833 - 1.17 min | 0.0139 - 0.0194 hour | per mm |
Amity Thermosets ATS 158 Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications:Switchgear componentCom.. |
|||
Cure Time | 0.833 - 1.33 min | 0.0139 - 0.0222 hour | per mm |
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |
|||
Cure Time | 0.833 - 1.33 min | 0.0139 - 0.0222 hour | per mm |
Amity Thermosets ATS 751 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:High impact strength Dimensional stabilityHigh mechanical strengthHeat stability ( 200°C )Good media resistance ( eg. Oil, water ) Low shrinkageGood electrical resistanceColor-brown.. |
|||
Cure Time | 0.833 - 1.33 min | 0.0139 - 0.0222 hour | per mm |
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R.. |