Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | >= 0.0833 min | >= 0.00139 hour | on metal (Fixture) |
ND Industries 624 Isopropyl Alcohol SuperGlue accelerator Very fast acting SuperGlue accelerator for plastic - 15 sec - Non-ozone depleting but flammable solvent |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Phenolic, handling time |
Permabond 101 Cyanoacrylate, Wicking Viscosity PERMABOND® 101 is a low viscosity product useful in wicking or penetrating applications or bonding closely fitting parts. It is fast setting and suitable for use on plastics, rubber and metals. Cya.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Buna N Rubber, handling time |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Phenolic, handling time |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | PVC, handling time |
Permabond 105 Cyanoacrylate, for difficult rubbers PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Steel, handling time |
Permabond 2011 Cyanoacrylate, gel PERMABOND® 2011 is a thixotropic, fast-setting cyanoacrylate particularly suitable for use on vertical and porous substrates. This material can be used on metals, plastics, elastomers, ceramics and.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Buna N Rubber, handling time |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Phenolic, handling time |
Permabond 268 Cyanoacrylate, General purpose PERMABOND® 268 is a medium-high viscosity cyanoacrylate for large gap fill applications. Permabond® 268 provides faster set times and improved gap-filling capability compared to conventional cyano.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Phenolic, handling time |
Permabond 735 Cyanoacrylate, toughened PERMABOND® 735 is a toughened cyanoacrylate with very good impact and peel strength when compared to a conventional cyanoacrylate. It bonds rapidly at room temperature and its viscosity is stable o.. |
|||
Cure Time | >= 0.0833 min | >= 0.00139 hour | Steel, set time |
Permabond QFS10 Cyanoacrylate Activator The PERMABOND QFS 10 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly.. |
|||
Cure Time | >= 0.0833 min | >= 0.00139 hour | Phenolic, set time |
Permabond QFS10 Cyanoacrylate Activator The PERMABOND QFS 10 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly.. |
|||
Cure Time | 0.0833 min | 0.00139 hour | fixture time, (low power 4mW lamp) |
Permabond UV620 UV-curable Adhesive PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I.. |
|||
Cure Time | 0.0833 min | 0.00139 hour | Phenolic, set time |
Permabond 260 Cyanoacrylate PERMABOND 260 is a low viscosity cyanoacrylate ideal for wicking type application. PERMABOND 260 provides faster set times and improved gap-filling capability compared to conventional cyanoacrylates.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Buna N Rubber, set time |
Permabond 931 Cyanoacrylate PERMABOND 931 is a low odor, nonfogging, nonfrosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Steel, set time |
Permabond 935 Cyanoacrylate The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | Buna N Rubber, set time |
Permabond 935 Cyanoacrylate The PERMABOND 930 series is a family of low odor, non-fogging, non-frosting cyanoacrylates. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyano.. |
|||
Cure Time | >= 0.0833 min | >= 0.00139 hour | Fixture |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Cure Time | >= 0.0833 min | >= 0.00139 hour | Fixture |
Resinlab® CYNERGY CA6801 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Cure Time | 0.0833 - 0.333 min | 0.00139 - 0.00556 hour | Plastic set time |
Lord Adhesives 9010 Medium Viscosity, Odorless, Non-Frosting Methoxyethyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Cure Time | 0.0833 min | 0.00139 hour | Hot tack |
Valley Adhesives EM-240 Low Temperature Application Glue Stick Valley Adhesives EM-240 Low Temperature Application Glue StickBonds many woods and wood composites; Excellent for woodworking and cabinetry. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | UV exposure |
Tra-Con Tra-Bond 546S05 Dual-Cure Acrylate TRA-BOND 546S05 is a dual cure (UV/heat) acrylate featuring excellent adhesion to glass. Ultimate Tg attained and shadowed areas cured with 15 minute exposure to 100-120°C.Information provided by T.. |
|||
Cure Time | 0.0833 - 0.250 min | 0.00139 - 0.00417 hour | 10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time. |
Dymax 9003v2.0 Hard Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v2.0 Hard Clear MicroencapsulantGlob top for photosensing devices Cure Type: UV/Visible Typical Use: Optical p.. |
|||
Cure Time | 0.0833 - 0.250 min | 0.00139 - 0.00417 hour | 10-20 mil thick layers cured with Dymax 5000-EC at 2 inches. Thicker layers may require more cure time. |
Dymax 9003v3.0 Flexible Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v3.0 Flexible Clear MicroencapsulantGlob top for photosensing devices Cure Type: UV/Visible Typical Use: Optic.. |
|||
Cure Time | <= 0.0833 min | <= 0.00139 hour | |
Dymax 9-318-F Peelable Mask High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-318-F Peelable MaskPeelable, wave solder resistant Cure Type: UV |
|||
Cure Time | <= 0.0833 min | <= 0.00139 hour | |
Dymax 955 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 955 Potting and Encapsulation AdhesiveHigh strength with superior adhesion to steel, aluminum and glass. Cure Type: .. |
|||
Cure Time | 0.0833 - 0.333 min | 0.00139 - 0.00555 hour | Time to Handling Strength |
3M Scotch-Weld™ MC100 Metal Instant Adhesive 3M™ Scotch-Weld™ Metal Instant Adhesives are designed to give optimum performance and high strength bonds on metals, including galvanized or anodized surfaces. MC100 (formerly SB30 or SB96) is a l.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling |
3M Scotch-Weld™ MG05 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |
|||
Cure Time | 0.0833 - 1.00 min | 0.00139 - 0.0167 hour | Time to Handling Strength |
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive 3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me.. |
|||
Cure Time | <= 0.0833 min | <= 0.00139 hour | Neoprene, handling time |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Cure Time | 0.0833 - 0.167 min | 0.00139 - 0.00278 hour | ABS, handling time |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |