Material Notes:
3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG05 LO is formulated to have low volatility means that these products are not only low volatility while maintaining bonding of a wide range of materials. Low volatility means that this product is not only low odor but also low blooming. Lower odor can improve worker comfort in applications where assembly requires being close to adhesive dispensing or where ventilation is limited. MG05 LO is useful for bonding very close-fitting parts and can be post-applied to assembled parts and allowed to wick into a bond lineInformation provided by 3M
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Viscosity 3.0 - 8.0 cP
3.0 - 8.0 cP
U-Tube IC-C45
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.1 MPa
1900 psi
cured, grit-blasted steel; ASTM D2095
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.0 °C
160 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Processing Properties Metric English Comments
Cure Time 0.0833 - 1.00 min
0.00139 - 0.0167 hour
Time to Handling
1440 min
24.0 hour
Full Cure
Descriptive Properties Value Comments
Appearance Clear Liquid