Polymer Property : Screw Speed = 100 rpm Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Screw Speed 50 - 100 rpm
50 - 100 rpm
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE)
Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene..
Screw Speed 40 - 100 rpm
40 - 100 rpm
Multibase Multi-Pro® 2003 TI Polypropylene
Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Screw Speed 40 - 100 rpm
40 - 100 rpm
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Screw Speed 50 - 100 rpm
50 - 100 rpm
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Screw Speed 70 - 100 rpm
70 - 100 rpm
LG Chemical Lupox® SV-1080 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Injection Molding
LG Chemical XR409E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
Screw Speed 60 - 100 rpm
60 - 100 rpm
Extrusion
Stellarchem MP-8001 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 60 - 100 rpm
60 - 100 rpm
Extrusion
Stellarchem SE/PA745B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP-2287C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP 1187 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP-1366A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® OBC 4876N Thermoplastic Elastomer
Uses: Flexible Grips; Overmolding; Soft Touch Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1081B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1402G Thermoplastic Elastomer
Notes: Non-halogenated, Flame Retardant TPE; RoHS Compliant Uses: Connectors; Electrical/Electronic Applications Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injec..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1488G Thermoplastic Elastomer
Uses: Flexible Grips; General Purpose; Handles; Household Goods; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast ..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Telcar® TL-2433A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol 66G33 2% Moly Nylon 66, 33% Glass Fiber Reinforced, 2% Molybdenum Disulfide Lubricated
Data provided by Clariant Masterbatches
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol BR7039G30 Nylon 6, 30% Glass Fiber, bondable to TPU
Data provided by Clariant Masterbatches
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol PA213G36S Nylon 6, 36% Glass Fiber, Heat Stabilized, Silicone Lubricated
Data provided by Clariant Masterbatches
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity
Data provided by Clariant Masterbatches
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol R66G13HSL Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Economy
Data provided by Clariant Masterbatches
Screw Speed 20 - 100 rpm
20 - 100 rpm
Clariant Renol 6608-L UV Black Nylon 66, High Impact Modified, Lubricated, UV Stable
Data provided by Clariant Masterbatches
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP-2840E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Screw Speed 50 - 100 rpm
50 - 100 rpm
Teknor Apex Monprene® MP-2875M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..