Processing Properties | Metric | English | Comments |
---|---|---|---|
Screw Speed | 80 - 160 rpm | 80 - 160 rpm | |
PolyOne Bergamid™ XP6042701 Polyamide 6 (Nylon 6) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3.5 sec Cycle Time: 18 to 60 secInformation provided by PolyOne |