Processing Properties Metric English Comments
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..