Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
PlastiComp Complet® LCF40 - PP Homopolymer Polypropylene, 40% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Star Plastics ABS3030 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP1192A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1458 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1566L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1579C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2137 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2228 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2241 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP 1097F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2860M-CR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-2870M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1000-95 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2519E Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-2683A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-4145A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-6800-73 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-83-F912-G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Back Pressure | 0.172 - 0.862 MPa | 25.0 - 125 psi | |
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |