Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This.. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Back Pressure | 15.0 - 25.0 MPa | 2180 - 3630 psi | Depending on wall thickness and part complexity |
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |