Processing Properties Metric English Comments
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC)
TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high ..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Back Pressure <= 15.0 MPa
<= 2180 psi
Specific
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Back Pressure 15.0 - 20.0 MPa
2180 - 2900 psi
Molding Pressure
Azoty Tarnow™ TARFLEN SM-1 PTFE
Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix
AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a ..
Back Pressure 15.0 - 25.0 MPa
2180 - 3630 psi
Depending on wall thickness and part complexity
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix
AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m..
Copyright © lookpolymers.com All Rights Reserved