Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G13P100-598UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (NH-293L) Seagull Gray Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP514-394 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 102E Medium Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products P256-01 Polypropylene Copolymer, Black Applications: Door/trunk scuffConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products T10P102-00EG 10% Talc Reinforced Polypropylene, Extrusion Grade, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products T10UP100-01 10% Talc Reinforced Polypropylene Copolymer, General Purpose Black, UL94 HB Rated Applications: Wire troughElectrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G20P100-601 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, (Ford ZUA5) Dark Graphite Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products G20P252-01 20% Glass Fiber Reinforced Polypropylene Copolymer, Black Applications: Interior trimArm rest insertConsolesDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP512-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Dry Time | 1 hour @Temperature 23.0 °C |
1 hour @Temperature 73.4 °F |
Prior to molding |
Lord Adhesives Chemlok® EP6964-07 Adhesive Chemlok® EP6964-07 is a water dilutable one-coat adhesive used to bond polyacrylates, polyacrylics, fluoroelastomers and silicones to metal during vulcanization.All information provided by Lord. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Dry Time | 1 hour | 1 hour | Predrying Time |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Dry Time | 1 hour | 1 hour | Predrying Time |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Dry Time | 1 - 2 hour | 1 - 2 hour | |
RheTech Products GC15P200-01 15% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Electrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |