Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 F1 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Potentially suitable for food/medical contact application. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 I8 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 L/07 Bio-Polymer Bio-Polymer (PLA, PHB, ...) based compound. Wood flour. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latilub 37 B01-02S Bio-Polymer Self-lubricating product based on Bio-Polymer (PLA, PHB, ...). Silicone.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Drying Temperature | 40.0 - 50.0 °C @Time 21600 sec |
104 - 122 °F @Time 6.00 hour |
|
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |