Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 65.0 - 102 °C | 149 - 216 °F | Average value: 71.5 °C Grade Count:7 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |