Processing Properties | Metric | English | Comments |
---|---|---|---|
Drying Temperature | 150 °C | 302 °F | |
PolyOne OnForce™ LFT SF-40LGF/001 Natural Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 170 °C | 302 - 338 °F | Always recommended, temperature can be reduced when using vacuum ovens. |
LATI LARPEEK 10 K/20 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Drying Temperature | 150 - 180 °C | 302 - 356 °F | Not necessary for reinforced materials. Temperature can be reduced when using vacuum ovens. |
LATI LAPEX A G/20 20% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Drying Temperature | 150 °C | 302 °F | 2.5 hours for injection molding |
Solvay Specialty Polymers Supradel® HTS-2401 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2401 is a high-temperature high-performance amorphous sulfone polymer designed for use in reinforced high temperature thermoplastic formulations. With its glass transition temperature o.. |
|||
Drying Temperature | 150 °C | 302 °F | 2.5 hours for injection molding |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Drying Temperature | 150 °C @Time 10800 - 18000 sec |
302 °F @Time 3.00 - 5.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1100-8325 Polyether sulfone, with glass fiber and PTFE Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.Improved friction and .. |
|||
Drying Temperature | 150 - 170 °C @Time 10800 sec |
302 - 338 °F @Time 3.00 hour |
|
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Drying Temperature | 150 °C @Time 10800 - 18000 sec |
302 °F @Time 3.00 - 5.00 hour |
Dehumidifying dryer |
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta.. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers KetaSpire® KT-880 GF15 Polyetheretherketone (PEEK), 15% Glass Fiber KetaSpire® KT-880 GF15 is a high flow, 15% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpi.. |
|||
Drying Temperature | 150 °C @Time 14400 sec |
302 °F @Time 4.00 hour |
|
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
Drying Temperature | 150 °C @Time 10800 sec |
302 °F @Time 3.00 hour |
|
Victrex® Vicote® 701 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |