Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced
Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13-[color]H Nylon, 13% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G20 Nylon 6, 20% Glass Reinforced
Nylon 6, 20% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G30 Nylon 6, 30% Glass Reinforced
Nylon 6, 30% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G33 Nylon 6, 33% Glass Reinforced
Nylon 6, 33% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G33-[color]-H Nylon 6, 33% Glass Reinforced, Heat Stabilized
Nylon 6, 33% Glass Reinforced, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G33-[color]H Nylon, 33% Glass Reinforced, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
Rear Barrel Temperature 249 - 268 °C
480 - 515 °F
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized