Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1 General Purpose Nylon 6 General Purpose Nylon 6, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP2 General Purpose Nylon 6, Nucleated General Purpose Nylon 6, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry .. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized General Purpose Nylon 6, Nucleated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1 Nylon 6, Impact Modified Nylon 6, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1-[color]-H Nylon 6, Impact Modified, Heat Stabilized Nylon 6, Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Rear Barrel Temperature | 221 - 246 °C | 430 - 475 °F | |
Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |