Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Multibase TPSiV® 4000-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SABIC HP7022 Low Density Polyethylene for Injection Molding Product Description: HP7022 is a Low Density Polyethylene offering a unique combination of consistent processability, flexibility and toughness. Articles manufactured from HP7022 exhibit excellent.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem FP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
Mold Temperature | 25.0 - 40.0 °C | 77.0 - 104 °F | Injection Molding |
Stellarchem MP-950NC TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Mold Temperature | 20.0 - 40.0 °C | 68.0 - 104 °F | |
SK Chemicals SKYTHANE® R180A Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Mold Temperature | 15.0 - 40.0 °C | 59.0 - 104 °F | |
Borealis RJ370MO Polypropylene, Transparent Random Copolymer RJ370MO is a specially modified highly-transparent polypropylene random copolymer with very high melt flow rate. It is designed for high-speed injection molding and contains nucleating and demoldin.. |
|||
Mold Temperature | 30.0 - 40.0 °C | 86.0 - 104 °F | |
Total LDPE 1200 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1200 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: flexible molding, handles, closures, household items, toys, variou.. |
|||
Mold Temperature | 10.0 - 40.0 °C | 50.0 - 104 °F | |
Borealis MG9601 Polyethylene MG9601 is a natural high-density polyethylene with high melt-index and narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. The grade is characterized by exce.. |