Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Gravi-Tech™ GRV-TE1-060-W-NAT Styrene Isoprene Styrene Block Copolymer (SIS) Information provided by PolyOne |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versaflex™ 9545-1 Thermoplastic Elastomer (TPE) Versaflex™ 9545-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ HC 9210-55N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-55N is a TPV alloy targeted for injection molding healthcare applications such as disposable medical items, syringe stoppers, and soft-touch overmolding onto surgical grips. Prod.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-70 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ XL 9045-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9045-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Versalloy™ XL 9055-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9055-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G7930-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE) Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7930-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. - NSF 51 approved - FDA (see Notes) - Overmold Adhesion to Polypropylene - Soft To.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Mold Temperature | 15.6 - 37.8 °C | 60.1 - 100 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Mold Temperature | 15.6 - 26.7 °C | 60.1 - 80.1 °F | |
PolyOne Dynalloy™ 8900-60 Thermoplastic Elastomer (TPE) Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylen.. |