Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 378 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 480 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 480P16 Glass Reinforced Engineering Resin Features:Very high modulus High heat resistance Excellent flow characteristics Excellent adhesion to urethaneApplications:Instrument panel substrates Consoles Cluster housings Interior trimInformati.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | |
Albis Plastics PC/PET 361E Unfilled
(discontinued **) Amorphous Polycarbonate /Polyethylene Terephthalate Blend (PC/PET)Characteristics: High Strength, Rigidity and Creep Resistance. Good Chemical ResistanceApplications: Pump Components, Industrial and.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | Cavity surface temp. at equilibrium |
NOVA Chemicals DYLARK® 250 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Mold Temperature | 54.0 °C | 129 °F | |
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 31% Plasticizer
(discontinued **) Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro.. |
|||
Mold Temperature | 54.0 - 71.0 °C | 129 - 160 °F | |
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber
(discontinued **) Data provided by PolyOne. |