Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 82.2 - 135 °C | 180 - 275 °F | |
PolyOne Gravi-Tech™ GRV-NY-035-SS-GF-BLK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Mold Temperature | 82.2 - 104 °C | 180 - 220 °F | |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Mold Temperature | 82.2 °C | 180 °F | |
Northstar Polymers MSS-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
PTS Tristar® PC-10R-CL(V6) 6 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 82.2 - 110 °C | 180 - 230 °F | |
PolyOne Edgetek® PS-30CF/000 Polybutylene Terephthalate (PBT), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Mold Temperature | 82.2 - 116 °C | 180 - 240 °F | |
Mitsubishi Iupilon® E2001R 5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Mold Temperature | 82.2 - 149 °C | 180 - 300 °F | |
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |