Polymer Property : Mold Temperature = 41.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A220-HT EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A220-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A240-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A240-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A240-ST EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A230-FRHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 49.0 °C
106 - 120 °F
Parker Chomerics PREMIER™ A230-HTHF EMI Shielding Plastic
Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer ..
Mold Temperature 41.0 - 100 °C
106 - 212 °F
Average value: 63.3 °C Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Mold Temperature 41.0 - 79.0 °C
106 - 174 °F
Albis Plastics ASA 02A 811 Unreinforced  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..
Mold Temperature 41.0 - 79.0 °C
106 - 174 °F
Albis Plastics ASA 02A MR20 , 20% Mineral Filled  (discontinued **)
Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel..