Processing Properties | Metric | English | Comments |
---|---|---|---|
Mold Temperature | 4.00 - 82.0 °C | 39.2 - 180 °F | Average value: 51.8 °C Grade Count:38 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Mold Temperature | 4.00 - 91.0 °C | 39.2 - 196 °F | Average value: 44.4 °C Grade Count:22 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Mold Temperature | 4.00 - 91.0 °C | 39.2 - 196 °F | Average value: 45.4 °C Grade Count:14 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |