Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3445D Thermoplastic Elastomer A NSF certified, high hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inje.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3445DN Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Nozzle Temperature | 188 - 221 °C | 370 - 430 °F | Injection Molding |
Teknor Apex Sarlink® 3490N Thermoplastic Elastomer A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4755A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® OBC 4864A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL EF-6155 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1025-85 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1336A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1431B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1520C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer Information Provided by Teknor Apex |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2363H Thermoplastic Elastomer Availability: North America Uses: Flooring; Furniture; General Purpose; Grommets; Textile Applications; Wire and Cable Applications Forms: Pellets Processing Method: Extrusion; Injection Molding In.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2555A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2570F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2572A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-2696A Thermoplastic Elastomer Uses: Cell Phones; Consumer Applications; General Purpose; Handles; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-87-L832A Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-88-N873K BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-91-T3056S-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-1996E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Nozzle Temperature | 188 - 210 °C | 370 - 410 °F | |
Teknor Apex Telcar® TL-8730R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |