Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | Injection molding |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | Injection molding |
Styrolution Styrolux 3G55 SBC Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex.. |
|||
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | Injection molding |
Styrolution Styrolux 656C SBC Styrolux 656C is a high flow thermoplastic injection molding styrene-butadiene block copolymer. It has crystal clarity, good toughness, good stiffness, and warpage resistance for general molding ap.. |
|||
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | Injection molding |
Styrolution Styrolux 684D SBC Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | |
Polyram Polytron P40B01 Homopolymer Polypropylene, Chemically Coupled 40% LGF A chemically coupled 40% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G45D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G45D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G90A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G90A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G90A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P75A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P75A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P80A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | >= 50.0 mm/sec | >= 1.97 in/sec | Injection |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Injection Velocity | 50.0 mm/sec | 1.97 in/sec | |
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind. |
|||
Injection Velocity | 50.0 - 75.0 mm/sec | 1.97 - 2.95 in/sec | |
Polyram Polytron A40B02 Nylon 66, 40% Long Fiber A 40% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |