Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8221-60 Thermoplastic Rubber
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 204 °C | 365 - 400 °F | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 185 - 195 °C | 365 - 383 °F | |
Huntsman AVALON® 75 AE Thermoplastic Polyurethane Introduction: AVALON 75 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 75 AE is part of the AVALON Soft Range and offers a premium soiling material .. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Metering zone |
Taiwan PU Corporation TPU-BH85 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Metering zone |
Taiwan PU Corporation TPU-CH95 High Hydrolysis Resistance, Calender Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Metering zone |
Taiwan PU Corporation TPU-E80 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Metering zone |
Taiwan PU Corporation TPUI-H85 High Hydrolysis Resistance, Injection Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Metering zone |
Taiwan PU Corporation TPUI-L85 Low Temperature Resistance, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-75 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8271-75 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 185 °C | 365 °F | Injection |
Alliance Polymers Viprene™ P70A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P70A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
(Unverified Data**) Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 191 °C | 365 - 375 °F | |
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-60 Thermoplastic Elastomer
(discontinued **) A soft, colorable, non-hygroscopic, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance .. |