Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 149 - 177 °C | 300 - 351 °F | |
PolyOne Dynaflex™ G6703-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6703-0001 is an easy processing compound designed for use in injection molding applications where extremely soft feel properties are desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Middle Barrel Temperature | 149 - 165 °C | 300 - 329 °F | |
Green Dot Terratek® Flex GDH-B1 Compostable Bioplastic Elastomer GDH-B1 is an elastomeric bioplastic with a diverse range of potential applications. It is a starch-based elastomer that is strong, durable and pliable with an exquisite soft touch. The bioplastic i.. |
|||
Middle Barrel Temperature | 149 °C | 300 °F | barrel 6 |
Borealis FR4845 Irradiation Crosslinkable Polyethylene Compound FR4845 is an Irradiation Crosslinkable non-halogen flame retardant compound developed for the automotive wire market. Applications: FR4845 is intended for use as a 125º C rated primary insulation .. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-001 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-005 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-026 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-082 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-190 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Middle Barrel Temperature | 149 - 218 °C | 300 - 425 °F | Injection molding cylinder temperature |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |