Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 290 - 330 °C | 554 - 626 °F | |
PolyOne Edgetek® XP9242701 Polyphenylene Sulfide (PPS) Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 secInformation provided by PolyOne |
|||
Middle Barrel Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA)
(Unverified Data**) Amodel AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temper.. |
|||
Middle Barrel Temperature | 316 - 330 °C | 601 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
Middle Barrel Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Middle Barrel Temperature | 320 - 330 °C | 608 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-4133 Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AE-4133 is a 33% glass reinforced, hot-water moldable polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Good Chemical Resistance; Good Cree.. |
|||
Middle Barrel Temperature | 316 - 330 °C | 601 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-8930 Polyphthalamide (PPA), 30% Glass Fiber Amodel® AE-8930 is a 30% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |
|||
Middle Barrel Temperature | 316 - 330 °C | 601 - 626 °F | |
Solvay Specialty Polymers Amodel® AE-8950 Polyphthalamide (PPA), 50% Glass Fiber Amodel® AE-8950 is a 50% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. Features: Glycol Resistant; Good Chemical Resistance; Good Creep .. |