Processing Properties Metric English Comments
Middle Barrel Temperature 154 - 171 °C
310 - 340 °F
RheTech Products E204-01 High Density Polyethylene, Black
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 160 - 171 °C
320 - 340 °F
Kleerdex Kydex® P51 Acrylic/PVC Extrusion Compound  (discontinued **)
Profile extrusion compound for building productsApplications: Handrails, crashrails, bumper guards, corner guardsFeatures: Extruded profiles made with P51 are extremely resistant to harsh chemicals ..
Middle Barrel Temperature 160 - 171 °C
320 - 340 °F
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound  (discontinued **)
High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel..
Middle Barrel Temperature 166 - 171 °C
330 - 340 °F
Kleerdex Kydex® P55 Acrylic/PVC Extrusion Compound  (discontinued **)
Weatherable profile extrusion compoundApplications: Extruded profiles requiring weatherability, high flexural modulus, and excellent flammability resistance. Features: Weatherability is dependent o..
Middle Barrel Temperature 154 - 171 °C
310 - 340 °F
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.