Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 190 °C | 374 °F | |
Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Middle Barrel Temperature | 190 °C | 374 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 7100 PRE-ELEC ESD 7100 is a static dissipative thermoplastic compound based on ABS. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7100 has been developed for inject.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HI100K ABS, High Impact Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical AF308 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
Middle Barrel Temperature | 190 - 240 °C | 374 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical SG175NS ABS, Super Surface Gloss, General Anti-Static Feature: Injection Molding, Super Surface Gloss, General Anti-StaticApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 °C | 374 °F | Compress zone |
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Middle Barrel Temperature | 190 °C | 374 °F | |
SK Chemicals SKYTHANE® S190A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis BB125MO Polypropylene Copolymer BB125MO is a heterophasic copolymer. This grade is a low melt flow rate grade intended for blow molding and sheet extrusion, and features extremely good process ability with improved melt strength a.. |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis RB307MO Polypropylene Random Copolymer RB307MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. This grade also features high heat distortion temperature. Applications: household and.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
Diamond Polymers ABS 1501 Description: Injection Molding GradeInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
Diamond Polymers ABS 4500R Description: Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
Diamond Polymers ABS VP-12 Description: Flame Retardant with UVInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
Diamond Polymers ABS 7501 Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 190 - 250 °C | 374 - 482 °F | |
Diamond Polymers ABS VP-11 Description: Flame Retardant ABSInformation provided by Diamond Polymers, Inc. |
|||
Middle Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer Zythane™ 5080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Middle Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Zythane™ 6080A Thermoplastic Polyurethane Elastomer Zythane™ 6080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |