Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10.0 - 30.0 min @Temperature 93.0 - 121 °C |
0.167 - 0.500 hour @Temperature 199 - 250 °F |
|
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Cure Time | 10.0 min @Temperature 121 °C |
0.167 hour @Temperature 250 °F |
Let sit for 24 hours to develop a final cure |
Lord Adhesives HPC-3C Fluoroelastomer Coating LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2000215D3 Silver / Silver Chloride Paste C2000215D3 has a ratio of Silver to Silver Chloride of 80/20. This is used for reference electrodes in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries. It forms part of a .. |
|||
Cure Time | 10.0 min @Temperature 125 °C |
0.167 hour @Temperature 257 °F |
|
Gwent Electronic Materials C2000904P3 Platinum Ink It can be used on partially stabilized zirconia and tape cast Materials. The Platinum powder contained within this paste has low shrinkage and high adhesion to ceramic substrates. Screen Printing E.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste.. |
|||
Cure Time | 10.0 min @Temperature 80.0 °C |
0.167 hour @Temperature 176 °F |
|
Gwent Electronic Materials C2050106D7 Carbon Graphite Ink This Carbon Graphite Ink is designed to be used for screen printing working electrodes. This is an ink which has been optimized to give superior electrochemical performance. It gives excellent elec.. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
box oven |
Gwent Electronic Materials C2061027P13 High Brightness Phosphor Ink (Blue/Green) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Cure Time | 10.0 min @Temperature 125 °C |
0.167 hour @Temperature 257 °F |
|
Gwent Electronic Materials C2071218D1 Gold Ink Gold Ink C2071218D1 is a fritted system that has been designed as a screen printing termination ink NTC components. It is also suitable for firing onto other high temperature substrates.This product.. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be .. |
|||
Cure Time | 10.0 min @Temperature 130 °C |
0.167 hour @Temperature 266 °F |
belt dryer |
Gwent Electronic Materials C2110817D5 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may b.. |
|||
Cure Time | 10.0 min @Temperature 125 °C |
0.167 hour @Temperature 257 °F |
|
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 330 Low Viscosity, Optical Epoxy Product Description: EPO-TEK® 330 is a two component, high-temperature grade, electrically and thermally insulating epoxy for semiconductor, electronics, fiber optics and medical applications.Advan.. |
|||
Cure Time | 10.0 min @Temperature 100 °C |
0.167 hour @Temperature 212 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® 353ND High Temperature Epoxy Product Description: EPO-TEK® 353ND is a two component, high temperature epoxy designed for semiconductor, hybrid, fiber optic, and medical applications. It is one of the most popular EPO-TEK® bra.. |
|||
Cure Time | 10.0 min @Temperature 150 °C |
0.167 hour @Temperature 302 °F |
|
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |
|||
Cure Time | 10.0 min @Temperature 120 °C |
0.167 hour @Temperature 248 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |
|||
Cure Time | 10.0 min @Temperature 175 °C |
0.167 hour @Temperature 347 °F |
|
Epoxyset Epoxiohm EO-38M-3 Electrically Conductive Epoxy Adhesive EO-38M-3 is a two components, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is used for thermal management appl.. |
|||
Cure Time | 10.0 min @Temperature 175 °C |
0.167 hour @Temperature 347 °F |
|
Epoxyset Epoxiohm EO-97M Electrically Conductive Epoxy Adhesive EPOXIOHM-97M is one part, pure silver filled, high electrical conductivity, epoxy adhesive. It is designed for microelectronics chip bonding application.Information provided by Epoxyset Inc. |
|||
Cure Time | 10.0 min @Temperature 50.0 °C |
0.167 hour @Temperature 122 °F |
|
Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning |
|||
Cure Time | 10.0 min @Temperature 204 °C |
0.167 hour @Temperature 399 °F |
|
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade) 3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate.. |
|||
Cure Time | 10.0 min @Temperature 150 °C |
0.167 hour @Temperature 302 °F |
|
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Cure Time | 10.0 min @Temperature 93.3 °C |
0.167 hour @Temperature 200 °F |
Step 1, preceeded by >10 min. air set |
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, brown-black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps.. |
|||
Cure Time | 10.0 min @Temperature 75.0 °C |
0.167 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Hyfro-Flex II PIR (Heat Reflective) Polyurethane Top Coat BLUE RIVER COATINGS HYDRO-FLEX II PIR POLYURETHANE TOPCOAT is a high performance, heat reflective, single component water dispersible polyurethane. HYDRO-FLEX II PIR is formulated with heat reflecti.. |
|||
Cure Time | 10.0 min @Temperature 93.3 °C |
0.167 hour @Temperature 200 °F |
Step 1, preceeded by >10 min. air set |
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, Jet Black coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, s.. |
|||
Cure Time | 10.0 min @Temperature 75.0 °C |
0.167 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as.. |