Cure Time 2.00 - 5.00 min

@Temperature 121 - 149 °C
0.0333 - 0.0833 hour

@Temperature 250 - 300 °F
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 2.00 - 5.00 min

@Temperature 121 - 149 °C
0.0333 - 0.0833 hour

@Temperature 250 - 300 °F
Lord Adhesives Chemglaze® V021 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 2.00 - 5.00 min

@Temperature 121 - 149 °C
0.0333 - 0.0833 hour

@Temperature 250 - 300 °F
Lord Adhesives Chemglaze® V175 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 3.00 - 5.00 min

@Temperature 150 °C
0.0500 - 0.0833 hour

@Temperature 302 °F
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..
Cure Time 2.00 - 5.00 min

@Temperature 121 - 149 °C
0.0333 - 0.0833 hour

@Temperature 250 - 300 °F
Lord Adhesives Chemglaze® V209 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 2.00 - 5.00 min

@Temperature 121 - 149 °C
0.0333 - 0.0833 hour

@Temperature 250 - 300 °F
Lord Adhesives Chemglaze® V300 Polyurethane Coating
Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m..
Cure Time 2.00 - 5.00 min

@Temperature 150 °C
0.0333 - 0.0833 hour

@Temperature 302 °F
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of..