Polymer Property : Cure Time = 480 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 480 - 960 min

@Temperature 25.0 °C
8.00 - 16.0 hour

@Temperature 77.0 °F
Resinlab® EP1285HD-16 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
Cure Time 480 min

@Temperature 82.2 °C
8.00 hour

@Temperature 180 °F
Complete Cure Cycle
Northstar Polymers MSB-D60A High Performance Polyurethane Cast Elastomer System
This is an Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires some lord bearing, high tensile strength, cut/tear res..
Cure Time 480 - 960 min

@Temperature 71.1 - 82.2 °C
8.00 - 16.0 hour

@Temperature 160 - 180 °F
Complete Cure Cycle
Northstar Polymers MSN-V40A Polyester Base Low-Rebound Impact/Vibration Dampening Gel
This polyurethane casting material is developed for applications that require Shore OO 40 range casting material with vibration dampening property and higher strength than standard polyurethane gel ..
Cure Time 480 min

@Temperature 93.3 °C
8.00 hour

@Temperature 200 °F
Lord Adhesives Thermosetâ„¢ LS 213-9 Unfilled Epoxy Encapsulant
Lord LS 213-9 is a one component epoxy coating and impregnating compound featuring low viscosity, good moisture resistance and excellent dielectric properties. Typical applications include transform..
Cure Time 480 min

@Temperature 60.0 °C
8.00 hour

@Temperature 140 °F
Tra-Con Tra-Bond 724-17GR Polyurethane Adhesive
TRA-BOND 724-17GR premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar..
Cure Time 480 min

@Temperature 75.0 °C
8.00 hour

@Temperature 167 °F
Tra-Con Tra-Bond 832-5 Flexible Epoxy
TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does no..
Cure Time 480 - 960 min

@Temperature 25.0 °C
8.00 - 16.0 hour

@Temperature 77.0 °F
Trelleborg Emerson & Cuming Eccobond® 1309 General Purpose Catalyst
Emerson & Cuming 1309 Eccobond® General Purpose CatalystFaster curing version of 9. Very fast room temperature curing, low viscosity, general purpose. Short working life. Imparts excellent chemical..
Cure Time 480 min

@Temperature 4.00 °C
8.00 hour

@Temperature 39.2 °F
Full Chemical
Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patc..
Cure Time 480 min

@Temperature 32.0 °C
8.00 hour

@Temperature 89.6 °F
Full Load
Chesterton ARC 988 Composite
Description: A high performance, quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by severe chemical and physi..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
Light Load
Chesterton ARC BX1 Sliding Wear Compound
Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
Light Load
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..
Cure Time 480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Overcoat Begin
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound
An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
Light Load
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite
Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
Tack Free
Chesterton MRS S4+ Metal Rebuilding System
An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375 microns (15 ..
Cure Time 480 - 720 min

@Temperature 25.0 °C
8.00 - 12.0 hour

@Temperature 77.0 °F
Epoxyset Epoxiohm EO-30FST Electrically Conductive Epoxy Adhesive
EO-30-FST is two part, fast cure, silver filled, and high electrical conductivity epoxy adhesive. Both components are silver filled permitting a simple 1:1 mix ratio by weight. It has smooth creamy ..
Cure Time 480 min

@Temperature 10.0 °C
8.00 hour

@Temperature 50.0 °F
Overcoat Begin
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating
Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with ..
Cure Time 480 min

@Temperature 16.0 °C
8.00 hour

@Temperature 60.8 °F
Tack Free
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating
Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with ..
Cure Time 480 min

@Temperature 4.00 °C
8.00 hour

@Temperature 39.2 °F
Full Chemical
Chesterton MRS 5 Metal Rebuilding System
MRS 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as we..
Cure Time 480 - 660 min

@Temperature 22.0 °C
8.00 - 11.0 hour

@Temperature 71.6 °F
Dow Corning 3-4241 DIELECTRIC TOUGH GEL KIT
Two-part, translucent green, RT or heat cure, UV indicator, long working time, tough primerless chemical adhesion, UL 94 V-1 flammability classification.Information provided by Dow Corning
Cure Time 480 min

@Temperature 5.00 °C
8.00 hour

@Temperature 41.0 °F
Dry to Handle Time; ASTM D1640 clause 7.7.1
3M Scotchkote™ 323 Purple Patch Compound
3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple..
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
demold time
BCC Products BC 8880 Polyurethane Elastomer Surface Coat
BC8880 is a two-part urethane gel coat which exhibits excellent handling characteristics and very low moisture sensitivity. Its characteristics include a high modulus and a high hardness. It is a br..
Cure Time 480 min

@Temperature 149 °C
8.00 hour

@Temperature 300 °F
Alternate
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.
Cure Time 480 min

@Temperature 60.0 °C
8.00 hour

@Temperature 140 °F
Tra-Con Tra-Bond 724-17GR1B3 Polyurethane Adhesive
TRA-BOND 724-17GR1B3 premixed and frozen polyurethane adhesive is designed for good adhesion, providing strong resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, myl..
Cure Time 480 - 840 min

@Temperature 24.0 °C
8.00 - 14.0 hour

@Temperature 75.2 °F
demold time
BCC Products BC 8675E Polyurethane Elastomer
BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
Tack Free
Chesterton ARC S4+ 100% Novolac acid resistant coating
Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. It is typically applied by spray, roller or brush at a nominal thickness of 375..
Cure Time 480 min

@Temperature 25.0 °C
8.00 hour

@Temperature 77.0 °F
3M AC-250 B-1/6 Aerospace Sealant
3M Aerospace Sealant AC-250 B-1/6 is a two-part, polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a thixotropic paste and can be read..