Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 - 480 min @Temperature 25.0 °C |
6.00 - 8.00 hour @Temperature 77.0 °F |
De-mold Time |
Northstar Polymers MPP-A47A Liquid Castable Polyurethane MPP-A47A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Cure Time | 360 min @Temperature 23.0 °C |
6.00 hour @Temperature 73.4 °F |
Stainless steel, handling strength |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Cure Time | 360 min @Temperature 23.0 °C |
6.00 hour @Temperature 73.4 °F |
Stainless steel, handling strength |
Permabond LH050 Anaerobic Threadsealant Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is .. |
|||
Cure Time | 360 min @Temperature 23.0 °C |
6.00 hour @Temperature 73.4 °F |
M10 steel, working strength |
Permabond LH050 Anaerobic Threadsealant Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is .. |
|||
Cure Time | 360 - 1440 min @Temperature 23.0 °C |
6.00 - 24.0 hour @Temperature 73.4 °F |
Zinc, working strength |
Permabond LH197 Anaerobic Gasketmaker Permabond® LH197 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is highly flexible, making it ideal for dissimilar surfaces where differential th.. |
|||
Cure Time | 360 - 1440 min @Temperature 23.0 °C |
6.00 - 24.0 hour @Temperature 73.4 °F |
Zinc, working strength |
Permabond LM012 Anaerobic Threadsealant Permabond® LM012 is an unfilled, medium viscosity anaerobic adhesive. Its major benefit as related to other pipe sealants is that it is an unfilled resin that is compatible with hydraulic fluids. I.. |
|||
Cure Time | 360 min @Temperature 23.0 °C |
6.00 hour @Temperature 73.4 °F |
Stainless steel, handling strength |
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u.. |
|||
Cure Time | 360 min @Temperature 23.0 °C |
6.00 hour @Temperature 73.4 °F |
Zinc, full strength |
Permabond MM115 Anaerobic Threadlocker Permabond® MM115 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and maintenance... |
|||
Cure Time | 360 min @Temperature 93.3 °C |
6.00 hour @Temperature 200 °F |
|
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°.. |
|||
Cure Time | 360 min @Temperature 25.0 °C |
6.00 hour @Temperature 77.0 °F |
Foot Traffic |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
Cure Time | 360 min @Temperature 32.0 °C |
6.00 hour @Temperature 89.6 °F |
Light Load/Overcoat End |
Chesterton ARC 982 100% Novolac acid resistant coating Description: An advanced polymer composite formulated to protect equipment from extreme chemical attack and corrosion. A low viscosity composite that is applied by brush, squeegee, or a plural compo.. |
|||
Cure Time | 360 min @Temperature 32.0 °C |
6.00 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC BX1 Sliding Wear Compound Description: An advanced contractor grade ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is normally applied at.. |
|||
Cure Time | 360 min @Temperature 32.0 °C |
6.00 hour @Temperature 89.6 °F |
Light Load |
Chesterton ARC HT-T Spark Testable High Temperature Trowelable Abrasion Control Compound An advanced ceramic composite formulated to protect equipment from corrosion and erosion in elevated temperature water solution immersion. This system is a high viscosity composite that is applied b.. |
|||
Cure Time | 360 min @Temperature 25.0 °C |
6.00 hour @Temperature 77.0 °F |
Tack Free |
Chesterton ARC PW Potable Water Coating Description: ARC PW is a 100% solids lining certified for NSF/ANSI 61 potable water, cold water service. It is recommended to be applied by brush, roll or spray at 500-750 microns (20-30 mils) total.. |
|||
Cure Time | 360 min @Temperature 60.0 °C |
6.00 hour @Temperature 140 °F |
|
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Cure Time | 360 min @Temperature 60.0 °C |
6.00 hour @Temperature 140 °F |
|
Cytec EN-2527 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Cure Time | 360 min @Temperature 60.0 °C |
6.00 hour @Temperature 140 °F |
|
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Cure Time | 360 min @Temperature 60.0 °C |
6.00 hour @Temperature 140 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Cure Time | 360 min @Temperature 45.0 °C |
6.00 hour @Temperature 113 °F |
Minimum Bond Line |
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr.. |
|||
Cure Time | 360 min @Temperature 25.0 °C |
6.00 hour @Temperature 77.0 °F |
Tack Free |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Cure Time | 360 min @Temperature 121 °C |
6.00 hour @Temperature 250 °F |
Alternate |
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound High Temperature, Low Viscosity, Low Expansion, High Glass Transition Temperature & Chemical Resistance |
|||
Cure Time | 360 - 480 min @Temperature 24.0 °C |
6.00 - 8.00 hour @Temperature 75.2 °F |
demold time |
BCC Products BC 8782 Urethane Casting BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi.. |
|||
Cure Time | 360 min @Temperature 107 °C |
6.00 hour @Temperature 225 °F |
|
Aremco Pyro-Putty™ 950 High Temperature Ceramic-Metallic Putty, Ceramic Fiber Filled Ceramic Fiber-Filled, Organic Caulk.For Sealing High Temperature Joints to 950°F.Cures Into a Tough, Pliable, Inert Material. |
|||
Cure Time | 360 min @Temperature 65.0 °C |
6.00 hour @Temperature 149 °F |
|
Parker Chomerics CHO-SHIELD® 596 A/B Silver-Epoxy Coating Silver-Epoxy Coating. This is a two-component, silver bearing, highly conductive epoxy paint designed to provide EMI shielding when applied to a dielectric substrate. It is also useful for coating f.. |
|||
Cure Time | 360 min @Temperature 32.0 °C |
6.00 hour @Temperature 89.6 °F |
Tack Free |
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating An advanced composite formulated to protect concrete and metal surfaces from corrosion and chemical attack. It is normally applied at a thickness of 1-2 mm (40-80 mils) per coat. However, greater si.. |