Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR14 NL MC PA6.6, 14% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 GR40 NL HS PA6.6, 40% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 GR30 NL MB PA6, 30% glass fiber reinforced, impact modified, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 GR15 NL HS PA6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecotek® PC30 NL VB03 PC, unfilled, UV stabilized, high impact, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecotek® PC40 NL VB02 PC, unfilled, UV stabilized, high impact, natural
Information provided by Eurotec® |
Hold Pressure |
50.0 - 100 MPa |
7250 - 14500 psi |
|
Eurotec® Tecomid® NB40 NL IH PA6, impact modified, natural
Information provided by Eurotec® |