Processing Properties Metric English Comments
Zone 5 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)  (Unverified Data**)
Veradel A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to st..
Zone 5 340 - 390 °C
644 - 734 °F
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer
Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s..
Zone 5 340 - 390 °C
644 - 734 °F
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer
Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc..
Zone 5 340 - 390 °C
644 - 734 °F
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer
Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re..
Zone 5 335 - 390 °C
635 - 734 °F
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..