Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 4 = 473 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 4 225 - 245 °C
437 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1063D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 235 - 245 °C
455 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 225 - 245 °C
437 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1163D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Zone 4 235 - 245 °C
455 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1172D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical
Zone 4 225 - 245 °C
437 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3047D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 225 - 245 °C
437 - 473 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3055D Ester Type TPE
Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Zone 4 230 - 245 °C
446 - 473 °F
Head
BASF Ultramid® HFX 33 PA6 (Dry)
Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
Zone 4 230 - 245 °C
446 - 473 °F
Head
BASF Ultramid® HFX 35 PA6 (Dry)
Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme..
Zone 4 230 - 245 °C
446 - 473 °F
Head
BASF Ultramid® HFX 37 PA6 (Dry)
Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en..
Zone 4 230 - 245 °C
446 - 473 °F
Head
BASF Nypel® 2351 HS BK PA6 (Dry)
Description: Nypel® 2351 HS BK is a heat stabilized, pigmented black, impact modified PA6 extrusion grade compound. Quality and performance are combines at a lower cost. It is based on recycled PA6..
Copyright © lookpolymers.com All Rights Reserved