Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 180 - 200 °C | 356 - 392 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 180 - 195 °C | 356 - 383 °F | Extrusion Molding |
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon. |
|||
Zone 4 | 180 °C | 356 °F | |
Borealis Borcell™ HE1123 High Density Polyethylene Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by.. |
|||
Zone 4 | 180 °C | 356 °F | Extrusion |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Zone 4 | 180 °C | 356 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Zone 4 | 180 °C | 356 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Zone 4 | 180 °C | 356 °F | |
Equate EFDC-7050 LLDPE Film Extrusion Resin EFDC-7050 is a linear low-density polyethylene resin for tubular blown film extrusion. Films extruded from EFDC-7050 have good toughness and high tensile strength and puncture resistance. The produc.. |