Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 175 - 205 °C | 347 - 401 °F | |
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Zone 4 | 185 - 205 °C | 365 - 401 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1030D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 4 | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-260D Thermoplastic Polyurethane ApplicationsExtrusion: Antenna, Heel TipInjection: Hose, Tube, SheetIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 4 | 195 - 205 °C | 383 - 401 °F | |
Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubr.. |
|||
Zone 4 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol. |
|||
Zone 4 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 4 | 195 - 205 °C | 383 - 401 °F | Injection |
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |