Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 225 - 245 °C | 437 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 Description: UBESTA has a strong resistance to chemicalsInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Ethylene Glycol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Nitric Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Water for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Calcium Chloride aq. for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sulfuric Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Trichloroethylene for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 - 250 °C | 437 - 482 °F | Middle |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 25 (2471) PA 6 Dry, 25% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 2 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 2 | 225 °C | 437 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Xylene for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |