Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 340 - 360 °C | 644 - 680 °F | |
Lehmann & Voss LUVOCOM® 1501/CF/30-1 Polysulfone, with carbon fiber Applications: Automotive industry, office machinery, medical- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Chemical and hydrolysis resistance parts, non.. |
|||
Zone 2 | 340 - 360 °C | 644 - 680 °F | |
Lehmann & Voss LUVOCOM® 1503-7986 Polysuper sulfone, with glass fiber and PTFE Applications: Automotive industry, office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved friction and w.. |