Polymer Property : Zone 1 = 302 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties with..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin
Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin
Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st..
Zone 1 140 - 150 °C
284 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/320 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/340 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a pol..
Zone 1 130 - 150 °C
266 - 302 °F
Fainplast Compounds HAX HF 200 Halogen Free PVC
HAX HF 200 is a thermoplastic flame retardant compound, and halogen free on polyolefinic basis. It can be used for the production of energy, signal and control cables
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Zone 1 130 - 150 °C
266 - 302 °F
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified  (discontinued **)
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi..
Copyright © lookpolymers.com All Rights Reserved