Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer Solvay Specialty Polymers
Trade Name Cogegum®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Cogegum® GFR/325 Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefin base containing a fire retardant system that contributes to give the cable self-extinguish properties without halogenidric acids evolution, toxic and corrosive gases and dark smoke emission.Features: Crosslinkable; Flame Retardant; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsAdditional Properties: Bending Test - IEC 60811 (-15°C): No cracks; Calorific Potential - ISO 1716 18.6 MJ/kg; Collar Temperature - 140 to 160 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 140 to 160 °C; Hot Air Shrinkage - IEC 60811 (100°C): < 4.0 %; Hot Pressure Test - IEC 60811 (100°C): < 50 %; Hot Set - IEC 60811 60 %; Hot Set - IEC 60811 0.0 %; Impact Test - IEC 60811 (-15°C): No cracks; Insulation Resistance Constant - IEC 60502 (20°C): 4000 Mohm·km; Insulation Resistance Constant - IEC 60502 (90°C): 20 Mohm·km; Temperature Index (Burning) - NES 715 300 °C; Water Absorption - IEC 60811 (100°C): < 1.00 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 6.2 g/10 min

@Load 21.6 kg,
Temperature 150 °C
6.2 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ISO 868
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 31 %
31 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+12 ohm-cm

@Temperature 90.0 °C
5.40e+12 ohm-cm

@Temperature 194 °F
ASTM D257
1.10e+15 ohm-cm

@Temperature 20.0 °C
1.10e+15 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Zone 2 130 - 150 °C
266 - 302 °F
Zone 3 140 - 160 °C
284 - 320 °F
Zone 4 140 - 160 °C
284 - 320 °F
Die Cooling Temperature 160 - 180 °C
320 - 356 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant