Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 1 = 195 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 1 175 - 195 °C
347 - 383 °F
Lubrizol Advanced Materials PEARLTHANE® 11T85E Thermoplastic Polyurethane Elastomer
Type: Pearlthane® 11T85E is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Extrusion/MouldingSpecial Features : Combining hardness with excellent mechanical pr..
Zone 1 180 - 195 °C
356 - 383 °F
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel..
Zone 1 175 - 195 °C
347 - 383 °F
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer
PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp..
Zone 1 185 - 195 °C
365 - 383 °F
Lubrizol Estane® X-595A-11 Thermoplastic Polyurethane
Type: Estane® X-595A-11 is a Shore 97A, polyester grade thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Extrusion.Available in AsiaInformation Provided by The Lubr..
Zone 1 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP85AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsInformation provided by Lubrizol.
Zone 1 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 1 185 - 195 °C
365 - 383 °F
Injection
Lubrizol ESTANE® GP92AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 92AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Zone 1 185 - 195 °C
365 - 383 °F
Eurostar Starpylen HU 30BF4 PP, 30% Bamboo Fiber Filled, Injection Molding
Starpylen HU30BF4 is a 30% Bamboo Fiber Reinforced Polypropylene Injection Molding Resin (also known as HU30BF4) (PRELIMINARY DATASHEET)Information provided by Eurostar.
Zone 1 185 - 195 °C
365 - 383 °F
Eurostar Starpylen HZ 30WF2 PP, 30% Wood Fiber Filled, Injection Molding
Starpylen HZ 30WF2 is a 30% Wood Fiber Reinforced Polypropylene Injection Molding Resin (also known as HZ30WF2)Information provided by Eurostar.