Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/TF/15/BK 100 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/30 Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/GF/10/TF/18/SI/2/GY5 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/TF/15/GY77 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-0957 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-1396 Polycarbonate, with carbon fiber, glass fiber and PTFE, electrically conducting Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7078/GY Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7216 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7289 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7289/V2 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7317 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-7856/FR/BK Polycarbonate, with carbon fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50-8300 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss ELECTRAFIL M-2386 Polycarbonate, with carbon fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 1 | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/GY Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |