Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 230 °C | 446 °F | Die |
Premix Thermoplastics PRE-ELEC® PP 1394 Conductive Thermoplastic Compound PRE-ELEC® PP 1394 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3020X25L Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: for coating steel and aluminumInformation provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030JLX2 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability Information provided by UBE. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Formic Acid (10%) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Fuel C for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Oil (ASTM D471 No. 1) for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Chloroform for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 °C | 446 °F | For 8x1 mm Tube Extrusion |
UBE UBESTA® 3030U Nylon 12 (After Sodium Hydroide for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 230 - 240 °C | 446 - 464 °F | |
Eurostar Staramide PF006IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF006IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X R2005-30V)Information provided by Eurostar. |