Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Die Temperature | 235 - 245 °C | 455 - 473 °F | |
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E671 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 3126 Adhesive Resin Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 39E660 Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 42E703 Adhesive Resin Bynel® Series 4200 resins are anhydride-modified low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E533 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont™ Bynel® 30E783 Anhydride Modified Ethylene Vinyl Acetate BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E850 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E871 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E662 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E739 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 50E806 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |
|||
Die Temperature | 235 °C | 455 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 12024S Ethylene Methyl Acrylate Elvaloy® AC 12024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Die Temperature | 235 °C | 455 °F | CoExtrusion with EVOH Processing |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 1707 Sodium Ionomer Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t.. |
|||
Die Temperature | 235 °C | 455 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® 2601B Sodium Ionomer Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer .. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 50E662 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E662 are based on polypropylene random copolymers. They are available in pellet form for use in conventional extrusion an.. |
|||
Die Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 50E631 Adhesive Resin
(discontinued **) Bynel® Series 5000 resins are anhydride-modified polypropylene. Bynel® 50E631 is based on polypropylene homopolymer. They are available in pellet form for use in conventional extrusion and coextru.. |