Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 190 - 205 °C | 374 - 401 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Inno-Comp INNOPOL® CS 1-7120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-7120 is a 20 % talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-7120 is recommended for extrusion of sheet.. |
|||
Die Temperature | 190 °C | 374 °F | |
Taiwan PU Corporation TPU-B85 General Grade, Blow Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Die Temperature | 190 °C | 374 °F | Body |
SK Chemicals SKYTHANE® CR180A Calendaring Series, Polyether Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1123 BLK 111 Thermoplastic Elastomer Uses: General Purpose; Grommets; Weather Stripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 1.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1154A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-150 BLK288 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Speci.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2478K Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2625C Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-83-F912-ER Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 227 °C | 374 - 440 °F | |
Teknor Apex Uniprene® UN-1069E2 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing Agency Ratings: UL 1581Forms: Pellets Processing Method: Extrusion; Injec.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-1996F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-86-K986-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Die Temperature | 190 - 210 °C | 374 - 410 °F | |
Teknor Apex Telcar® TL-8732 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |